SPECIFICATION

TestMethode40-5060-70 (1)60-70 (2)*80-100*85-100100-120
DensityASTM D-71/01-1/061/01-1/06>0.991.00-1.051/01-1/051/01-1/04
Penetration Rate at 25 CASTM D-540-5060-7060-7080-10085-100100-120
Softening Point CASTM D-3652-6049-5646<4245-5242-49
Ductility at 25 C (cm)ASTM D-113100 Min100 Min100> 100100 Min100 Min
Flash Point CASTM D-92250 Min250 Min240< 225250 Min250 Min
Solubility in disulfide %wtASTM D-499/599/5--------99/599/5
Stain testAASHTO T 102negativenegative--------negativenegative
weight loss by heating %wtASTM D-60/2 Max0/2 Max1 Max< 0.50/2 Max0/2 Max
penetration loss by heating %ASTM D-6-D-520 max20 max--------20 max20 max
Solubility in TCE MinASTM D 2042--------99> 99.05--------
Increase in Softening point maxASTM D 36--------10------------